Qijia Classroom: How to Prevent and Solve the Problem of 12 Large Wall Construction Problems


   Nippon Paint (Western Chemicals)  

1, coating wrinkling

Cause: The application of too thick, wet film drying time is not enough, suddenly high temperature accelerated drying.

Prevention: 1 thin coating; 2 appropriate extension of time; 3 to prevent the wet film heating up too quickly.

Solution: Recoat the paint after it has been leveled.

Blistering

Reasons: 1 under direct sunlight or the substrate is hotter; 2 wet when the substrate is wet; 3 moisture escapes from the interior through the external wall; 4 exposed to high humidity environment; 5 short-term drying after the film maintenance within the rain.

Prevention: 1 Confirm that the humidity of the substrate is less than 10%; 2 Confirm the recoating time, according to the time required by the product; 3 In the hot weather in the summer, avoid construction at noon.

Solution: Determine if blisters occur on the substrate, locate and remove the source, scrape blisters, and repaint.

3, cracking, peeling

Reasons: 1 use of inferior paint; 2 excessive dilution or coating too thick; 3 improper surface treatment, such as putty is too thick, loose, poor durability; 4 cracking of the paint film caused by the cracking of the substrate; 5 paint is too hard or due to age Aging becomes brittle.

Prevention: 1 use high-quality paint; 2 multi-layer peeling, use putty.

Solution: Brush off loose materials, sand the surface, sand edges; use as little putty with a certain durability and water resistance.

4, foaming / shrinkage

Reasons: 1 excessive vibration barrel; 2 using two different qualities of paint or coating time is too long; 3 roller coating is too fast; 4 roller hair is too long; 5 coating is repeatedly roller coating or brush back and forth; 6 in the porous The surface roller is coated with light or matte paint.

Prevention: 1 use high-quality paint; 2 keep it for a period of time before brushing, so that the paint eliminates bubbles caused by dilution, stirring and vibration; 3 avoid excessive repetitive roller coating or brushing; 4 use short hair rollers ;5 Use a primer on the porous surface first.

Solution: Recoat after grinding.

Wall construction three trees paint paint paint latex paint bathroom room

1 23 Next> Total 3 Pages
Page to page
Function assignPage() { var page = $('#page_val').val(); if (/_\d+\.html$/.test(location.href)) { location.href = location.href.replace( /_\d+\.html/, ((page == 1) && 1? '' : '_' + page) + '.html') } else if(/\/\d+\.html$/.test (location.href)) { location.href = location.href.replace(/(\d+)\.html/, ((page == 1) && 1? '$1' :'$1_' + page) + ' .html') } } $(function(){ $('#page_form').submit(function() { assignPage() return false; }) $('#page_btn').click(function(){ assignPage( ); return false; }) }) See full story

Bread Basket

Bread basket,stainless wire basket,stainless wire bread basket,Metal Wire Bread Basket,steel bread basket,etc. we offered that you can trust. Welcome to do business with us.

Kichen Rack is made of high quality 304 stainless steel, This kind of material steel luxury, never rust, resist corruption, easily clean, safe, healthy and durable. Prevent rust or chemicals from contaminating food and damaging health

stainless wire basket,stainless wire bread basket,Metal Wire Bread Basket,steel bread basket,versatile basket

Shenzhen Lanejoy Technology Co.,LTD , https://www.wirefruitbasket.com